[1] Ikeda Y, Kohjiya S. Chemistry, manufacture and applications of natural rubber[M].Cambridge: Woodhead,2014:3-21.[2] Schultes R E. Natural rubber science and technology [J]. Economic Botany,1991(1):139-140.[3] Webster C C, Baulkwill W J. Rubber[M]. London:Longman Scientific & Technical,1989:238-243.[4] Sethuraj M R, Mathew N M. Natural rubber: Biology, cultivation and technology[M]. Holland:Elsevier Science,1992:1-20.[5] Seentrakoon, Boonchai, Chavasiri. Enhanced UV-protection and antibacterial properties of natural;rubber/rutile-TiO2 nanocomposites[J]. Polymer Degradation & Stability,2013,98(2):566-578.[6] Huang Menglong, Guibert M, Thevenet J, et al. A new test method to simulate low-severity wear conditions experienced by rubber tire materials[J]. Wear,2018,410:72-82.[7] Marco Y, Huneau B, Masquelier I, et al. Prediction of fatigue properties of natural rubber based on the descriptions of the cracks population and of the dissipated energy [J]. Polymer Testing 2017,59:67-74.[8] Shimada K, Saga N. Development of a hybrid piezo natural rubber piezoelectricity and piezoresistivity sensor with magnetic clusters made by electric and magnetic field assistance and filling with magnetic compound fluid [J]. Sensors,2017,17(2):346.[9] Spratte T, Plagge J, Wunde M, et al. Investigation of strain-induced crystallization of carbon black and silica filled natural rubber composites based on mechanical and temperature measurements[J]. Polymer,2017,115:12-20.[10] Borges F A, De Barros N R, Garms B C, et al. Application of natural rubber latex as scaffold for osteoblast to guided bone regeneration [J]. Journal of Applied Polymer Science,2017,134(39):45321.[11] Siregar A M, Wirjosentono B, Eddiyanto, et al. Oxidation degradation analysis of cyclic natural rubber (resiprene-35) due to storage, heating and ultraviolet rays [J]. Siregar,2016,8(8):100-111.[12] Baldwin J M, Bauer D R, Ellwood K R. Rubber aging in tires(Part 1): Field results[J]. Polymer Degradation and Stability,2007,92(1):103-109.[13] Wang Weizhi, Qu Baojun. Photo- and thermo - oxidative degradation of photocrosslinked ethylene-propylene-diene terpolymer [J]. Polymer Degradation & Stability,2003,81(3):531-537.[14] Nor H M, Ebdon J R. Telechelic liquid natural rubber: A review [J]. Progress in Polymer Science,1998,23(2):143-177.[15] Shera M, Siby V, Rani J. Degradation behaviour of natural rubber layered silicate nanocomposites [J]. Progress in Rubber, Plastics and Recycling Technology,2013,29(1):1-19.[16] 杨小田,张博,康建铭,等.橡胶老化及其防护技术的研究概况[J]. 化工管理,2020(20):100-101.[17] 雷卫华,王建华,田野. MVQ-EPDM并用胶及泡沫的热老化性能研究[J]. 特种橡胶制品,2005(3):16-18.[18] Kutschke K O. Photochemistry [J]. Journal of the Franklin Institute,1967,284(2):147-148.[19] Allen N S. Recent advances in the photo-oxidation and stabilization of polymers [J]. Chemical Society Reviews,1986,15(3):373-404.[20] Morton M. Introduction to rubber technology[M]. NewYork: Chapman and Hall,1959:169-171.[21] Kurian J K, Peethambaran N R, Mary K C, et al. Effect of vulcanization systems and antioxidants on discoloration and degradation of natural rubber latex thread under UV radiation [J]. Journal of Applied Polymer Science,2015,78(2):304-310.[22] Ibrahim S, Othman N, Ismail H. Degradation of natural rubber latex[J]. Natural Rubber: Properties, Behavior and Applications,2016,21:105-136.[23] Ravindran T, Nayar M R G, Francis D J. Production of hydroxyl-terminated liquid natural rubber—mechanism of photochemical depolymerization and hydroxylation[J]. Journal of Applied Polymer Science,2010,35(5):1227-1239.[24] Santos K A M D, Suarez P A Z, Rubim J C. Photo-degradation of synthetic and natural polyisoprenes at specific UV radiations [J]. Polymer Degradation and Stability,2005,90(1):34-43.[25] Ravindran T, Nayar M R G, Francis J D. A novel method for the preparation of hydroxyl terminated liquid natural rubber [J]. Macromolecular Rapid Communications,1986,7(3):159-163.[26] Tasakorn P, Amatyakul W. Photochemical reduction of mole-cular weight and number of double bonds in natural rubber film [J]. Korean Journal of Chemical Engineering,2008,25(6):1532-1538.[27] Chaikumpollert O, Sae-Heng K, Wakisaka O, et al. Low temperature degradation and characterization of natural rubber [J]. Polymer Degradation and Stability,2011,96(11):1989-1995.[28] Ibrahim S, Othman N, Nor Z M, et al. Preliminary study on photochemical degradation of natural rubber latex [J]. Macromolecular Symposia,2017,371(1):22-26.[29] Riyajan S A, Sakdapipanich J T, Tanaka Y. Controlled degradation of cured natural rubber by encapsulated benzophenone as a photosensitizer [J]. Journal of Applied Polymer Science,2010,90(1):297-305.[30] 刘丽园. 两种胺类防老剂对天然橡胶热氧老化防护机理的实验及分子模拟研究[D]. 北京:北京化工大学,2018.[31] Morand J. Chain scission in the oxidation of polyisoprene[J]. Rubber Chemistry and Technology,1977,50(2):373-396.[32] Yano S. Photo-oxidation of an IR vulcanizate [J]. Rubber Chemistry and Technology,1981,54(1): 1-14.[33] Zhang Fuquan, Huang Maofang, Chen Mei, et al. Thermal-oxidation degradation of microwave drying nature rubber[J]. Advanced Materials Research,2012,399:1600-1603.[34] 丁玲. 天然橡胶和异戊橡胶老化研究[D]. 厦门:厦门大学,2018.[35] Martin J W, Chin J W, Nguyen T. Reciprocity law experiments in polymeric photodegradation: A critical review [J]. Progress in Organic Coatings,2003,47(3):292-311.[36] Zhao Quanlin, Li Xiaogang, Gao Jin. Surface degradation of ethylene-propylene-diene monomer (EPDM) containing 5-ethylidene-2-norbornene (ENB) as diene in artificial weathering environment [J]. Polymer Degradation and Stability,2008,93(3):692-699.[37] Thomas R. Kirk-othmer encyclopedia of chemical technology(part II): Antioxidants, polymers [M]. NewYork: John Wiley,2000:10-20.[38] Shahidi F, Janitha P K, Wanasundara P D. Phenolic antioxidants[J]. Critical Reviews in Food Science and Nutrition,1992,32(1):67-103.[39] Xin Cuiping. Development and application of phosphite antio-xidant [J]. Yunnan Chemical Technology,2004,31:15-18.[40] 张朋朋. 防老剂在橡胶中的应用性能评价研究[D]. 北京:北京化工大学,2014.[41] 刘凯凯,陈俊,郭绍辉. 新型防老剂RT-1对天然橡胶性能的影响[J]. 橡胶工业,2014,61(11):676-679.[42] 穆洪帅,刘权,谭莲影,等. 配合体系对NR长期热空气老化性能的影响[J]. 世界橡胶工业,2016,43(10):25-29.[43] Edge M, Allen N S, Gonzalez-Sanchez R, et al. The influence of cure and carbon black on the high temperature oxidation of natural rubber(part I):Correlation of physico-chemical changes[J]. Polymer Degradation and Stability,1999,64(2):197-205.[44] Rao S, Devi S N S, Johns A, et al. Mechanical and thermal properties of carbon black reinforced natural rubber/polyvinyl alcohol fully-interpenetrating polymer networks[J]. Journal of Vinyl and Additive Technology,2018,24:21-29.[45] Wen Xin, Wang Yujie, Gong Jiang, et al. Thermal and flammability properties of polypropylene/carbon black nanocomposites [J]. Polymer Degradation and Stability,2012,97(5):793-801.[46] Zeynalov E B, Allen N S, Salmanova N I. Radical scavenging efficiency of different fullerenes C 60-C 70 and fullerene soot [J]. Polymer Degradation and Stability,2009,94(8):1183-1189.[47] Galano A. Carbon nanotubes as free radical scavengers [J]. Journal of Physical Chemistry,2008,112(112):8922.[48] Yang Julong, Huang Yajiang, Lv Yadong, et al. The synergistic mechanism of thermally reduced graphene oxide and antioxidant in improving the thermo-oxidative stability of polypropylene [J]. Carbon,2015,89(5):340-349.[49] Troitskii B B, Troitskaya L S, Dmitriev A A, et al. Inhibition of thermo-oxidative degradation of poly(methyl methacrylate) and polystyrene by C 60 [J]. European Polymer Journal,2000,36(5):1073-1084.[50] Bocchini S, Blasio A D, Frache A. Influence of MWNT on polypropylene and polyethylene photooxidation [J]. Macromolecular Symposia,2011,301(1):16-22.[51] Ismail H, Ramly A F, Othman N. The effect of carbon black/multiwall carbon nanotube hybrid fillers on the properties of natural rubber nanocomposites[J]. Journal of Macromolecular Science(Part D):Reviews in Polymer Processing,2011,50(7):660-666.[52] Bokobza L, Rahmani M, Belin C, et al. Blends of carbon blacks and multiwall carbon nanotubes as reinforcing fillers for hydrocarbon rubbers [J]. Journal of Polymer Science(Part B ):Polymer Physics,2010,46(18):1939-1951.[53] Das A, Wang Deyi, St■ckelhuber K W, et al. Rubber-clay nanocomposites: Some recent results[J]. Advanced Rubber Composites,2010,239:85-166.[54] Reowdecha M, Sukthaworn C, Dittanet P, et al. Degradation of silica-reinforced natural rubber by UV radiation and humidity in soil [J]. Key Engineering Materials,2017,751:314-319.[55] Amnuaypornsri S, Kawahara S, Toki S, et al. Strain-included crystallization of un-vulcanized natural rubber measured by synchrotron X-ray diffraction [J]. Kautschuk Gummi Kunststoffe,2012,65(6):46-50.[56] Wu Jinrong, Qu Wei, Huang Guangsu, et al. Super-resolution fluorescence imaging of spatial organization of proteins and lipids in natural rubber [J]. Biomacromolecules,2017,18(6):1705-1712.[57] Chaikumpollert O, Yamamoto Y, Suchiva K, et al. Protein-free natural rubber[J]. Colloid and Polymer Science,2011,290(4):331-338.[58] Zhou Yuanbing, Kosugi K, Yamamoto Y, et al. Effect of non-rubber components on the mechanical properties of natural rubber [J]. Polymers for Advanced Technologies,2017,28(2):159-165.[59] Abad L V, Relleve L S, Aranilla C T, et al. Natural antioxidants for radiation vulcanization of natural rubber latex[J]. Polymer Degradation and Stability,2002,76(2):275-279.[60] Tuampoemsab S, Sakdapipanich J. Role of naturally occuring lipids and proteins on thermal aging behaviour of purified natural rubber[J]. Kautschuk Gummi Kunststoffe,2007,60(12):678-684.