|本期目录/Table of Contents|

[1]李世昆,王洪振,周海月,等.复合型增强剂对氢化丁腈橡胶/氟橡胶复合材料性能的影响[J].合成橡胶工业,2023,3:215-220.
 LI Shi-kuna,WANG Hong-zhena,ZHOU Hai-yueb,et al.Effect of composite reinforcing agents on the properties of HNBR/FKM composites[J].China synthetic rubber industy,2023,3:215-220.
点击复制

复合型增强剂对氢化丁腈橡胶/氟橡胶复合材料性能的影响(PDF)

《合成橡胶工业》[ISSN:1000-1255/CN:62-1036/TQ]

期数:
2023年3期
页码:
215-220
栏目:
出版日期:
2023-05-15

文章信息/Info

Title:
Effect of composite reinforcing agents on the properties of HNBR/FKM composites
文章编号:
1000-1255(2023)03-0215-06
作者:
李世昆1王洪振1周海月2杜正鹏2蔡荣强2李道壮2李再峰2?鄢
1. 青岛科技大学 橡塑材料与工程教育部重点实验室; 2. 化学与分子工程学院,山东 青岛 266042
Author(s):
LI Shi-kuna WANG Hong-zhena ZHOU Hai-yueb DU Zheng-penga CAI Rong-qiangb LI Dao-zhuangb LI Zai-fengb
a. Key Laboratory of Rubber-Plastic of Ministry of Education, Ministry of Education;b. College of Chemistry and Molecular Engineering, Qingdao University of Science and Technology, Qingdao 266042, China
关键词:
复合型增强剂氢化丁腈橡胶氟橡胶复合材料物理机械性能动态力学性能耐热氧老化性能
Keywords:
composite reinforcing agent hydrogenated nitrile rubber fluororubber composite physico-mechanical properties dynamic mechanical property thermal-oxydative aging property
分类号:
TQ 330.1+5
DOI:
DOI:10.19908/j.cnki.ISSN1000-1255.2023.03.0215
文献标识码:
B
摘要:
将炭黑(CB)、氢氧化单甲基丙烯酸锌(HZMMA)和碳纳米管(CNTs)进行复配,以改性氢化丁腈橡胶(HNBR)/氟橡胶(FKM)共混胶,制备了HNBR/FKM复合材料,研究了复合型增强剂对HNBR/FKM共混胶硫化特性、硫化胶的物理机械性能、动态力学性能和耐热氧老化性能的影响。结果表明,当加入HZMMA和CNTs后,HNBR/FKM复合材料的硫化速率加快且交联程度提高;在HZMMA和CNTs的协同作用下,HNBR/FKM复合材料的物理机械性能明显提高;与纯CB增强的相比,加入3份(质量)CNTs的HZMMA增强的HNBR/FKM复合材料热氧老化后扯断伸长率的保持率最高,与此同时硬度变化率最低;随着CNTs添加量的增加,HNBR/FKM复合材料的玻璃化转变温度向低温方向移动,同时损耗因子呈逐渐下降的趋势。
Abstract:
HNBR/FKM composites were prepared by compounding carbon black (CB), hydroxide zinc monomethacrylate (HZMMA) and carbon nanotubes (CNTs) to modify hydrogenated nitrile rubber (HNBR)/ fluororubber (FKM) blend, and the effects of the composite reinforcing agent on the curing characteristics of HNBR/FKM blends, and the physico-mechanical properties, dynamic mechanical properties and thermal-oxydative aging properties of the vulcanized rubber were investigated. The results showed that the curing rate of HNBR/FKM compo-sites was accelerated and the cross-linking degree was increased when HZMMA and CNTs were added, and the physico-mechanical properties of HNBR/FKM composites were significantly improved under the synergistic effect of HZMMA and CNTs. HNBR/FKM composites reinforced by HZMMA and CNTs of 3 phr (mass) exhibited the highest retention rate of elongation at break and the lowest change rate of hardness after thermal-oxydative aging compared with that reinforced by pure CB. As the addition amount of CNTs increased, the glass transition temperature of HNBR/FKM composites moved towards the lower temperature and the loss factor decreased gradually.

参考文献/References

[1] Guo Jianhua, Chen Xuming, Li Zhicai. Thermal oil aging behavior of hydrogenated nitrile butadiene rubber/multi-walled carbon nanotube composites under free or compression state[J]. Journal of Elastomers & Plastics, 2018, 50(5): 448-462.[2] Kommling A, Jaunich M, Wolff D. Effects of heterogeneous aging in compressed HNBR and EPDM O-ring seals[J]. Polymer Degradation and Stability, 2016, 126: 39-46.[3] Xie Hongquan, Li Xiaodong, Guo Junshi. Hydrogenation of nitrile-butadiene rubber latex to form thermoplastic elastomer with excellent thermooxidation resistance[J]. Journal of applied polymer science, 2003, 90(4): 1026-1031.[4] 李明晏, 张磊, 李会雨. 氟橡胶高温下力学性能试验研究[J]. 科技风, 2013(7): 9.[5] 亓明, 贾现召, 石建永, 等. 不同填料氟橡胶复合材料高温性能研究[J]. 润滑与密封, 2021, 46(2): 106-113.[6] 谢尊虎. 耐高温耐油硅橡胶共混材料的制备与性能研究[D]. 青岛: 青岛科技大学, 2012.[7] 李东翰, 廖明义. 氟橡胶在碱性环境中脱氟化氢反应机理及其结构[J]. 材料导报, 2018, 32(10): 1730-1736.[8] Mashita R, Kishimoto H, Inoue R, et al. Dynamics of polybutadiene reinforced with unsaturated carboxylate studied by muon spin relaxation (μSR)[J]. Polymer, 2016, 105: 510-515.[9] Mashita R, Kishimoto H, Inoue R, et al. Small-angle X-ray and neutron scattering analyses of highly crosslinked rubber with unsaturated carboxylic acid[J]. Polymer Journal, 2013, 45(1): 57-63.[10] 王冠中, 田帅承, 刘红天,等. 单甲基丙烯酸锌增强丁腈及氢化丁腈橡胶复合材料的热氧老化研究[J]. 化学工程师, 2015, 29(7): 1-4.[11] 王增林, 马珍福, 陈静哲,等. 单甲基丙烯酸锌改性氢化丁腈橡胶老化过程的力学性能演变及其老化动力学[J]. 合成橡胶工业, 2019, 42(3): 204-208.[12] 王琦, 刘勋聪, 马原, 等. 碳纳米管增强天然橡胶/反式-1,4-聚异戊二烯形状记忆复合材料的性能[J].合成橡胶工业, 2022, 45(1): 40-44.[13] 赵艳芬, 苏正涛, 王珊, 等. 碳纳米管增强HNBR橡胶及其对橡胶性能的影响[J]. 弹性体, 2020, 30(3): 41-45.[14] 向宇, 吴俊, 张晓辉, 等. 碳纳米管在氢化丁腈橡胶密封制品中的应用[J]. 橡胶科技, 2019, 17(8): 462-466.[15] Zhang Zeng, Li Hui, Zhou Haiyue, et al. Modification and improvement of aging resistance for HNBR/graphite composites[J]. Journal of Macromolecular Science (Part A): Pure and Applied Chemistry, 2022: 1-10.[16] Wu Siwu, Weng Peijin, Tang Zhenghai, et al. Sustainable carbon nanodots with tunable radical scavenging activity for elastomers[J]. ACS Sustainable Chemistry & Engineering, 2016, 4(1): 247-254.[17] Xu Xiang, You Yang, Liu Xingyu, et al. Experimental and density functional theory investigations on the antioxidant mechanism of carbon nanotubes[J]. Carbon, 2021, 177: 189-198.[18] Li Hui, Cheng Kai, Zhang Zeng, et al. Effect of carbon nanotubes on aging properties of hydrogenated nitrile rubber in the dilute oxygen medium[J]. Journal of Macromolecular Science (Part A): Pure and Applied Chemistry, 2021: 1-8.[19] 陈竞哲, 王建海, 张潇, 等. 氢化丁腈橡胶/氟橡胶复合材料的相容性、力学性能及热氧老化性能[J].合成橡胶工业, 2018, 41(4): 261-265.[20] 李继新, 徐祥明. HNBR/FKM橡胶密封筒用料的制备及力学性能表征[J]. 橡塑技术与装备, 2017, 43(3): 34-38.[21] Drozdov A D, Dorfmann A. The Payne effect for particle‐reinforced elastomers[J]. Polymer Engineering & Science, 2002, 42(3): 591-604.